Details: in-situ reconditioning of worn-out cms (cast manganese steel) crossings of all types, as per reconditioning manual and "work procedure for in-situ reconditioning of cms crossing using robotic welding machine" of rdso, through approved agency, finishing & grinding within permissible tolerance limit, as directed by engineer in-charge. note: reconditioned crossing shall have guaranteed service life of minimum 80 gmt. in case of pre-mature reconditioning, it shall be done by the contractor free of cost. reconditioning of worn out 1:8½ tongue rail (only one tongue rail along with connected stock rail) of all rail sections on cess or depot, as prescribed in 'ir's reconditioning of points & crossings manual' with rdso approved electrodes of h3 c electrodes, finishing & grinding within permissible tolerance limit, as directed by engineer in-charge. note: the work shall be carried out with proper welding, finishing and grinding to match with the existing rail top surface. cutting of 52kg / 60kg