Details: demolishing brick work manually/ by mechanical means including stacking of serviceable material and disposal of unserviceable material within 50 metres lead as per direction of engineer-in charge. 3.1.1 in cement mortar carriage of materials by mechanical transport including loading, unloading and stacking ::earth sand, bazri, ballast, kankar for 2 km providing and laying lean cement concrete 1:4:8 in sub- base over a prepared sub-grade with coarse and fine aggregate conforming to is: 383, the size of coarse aggregate not exceeding 25 mm, aggregate cement ratio not to exceed 15:1, aggregate gradation after blending to be as per table 600-1, cement content not to be less than 150 kg/ , optimum moisture content to be determined during trial length construction, concrete strength not to be less than 10 mpa at 7 days, mixed in concrete mixer, laid manually, compacted with surface , finishing and curing complete as per clause 601, 112 of mort&h specification including all material, labou